  • Reviews

Operating Environment

  • Indoor Temperature: 25°C
  • Humidity: 60%-70%

Resin Types

  • A Resin: Liquid, Translucent Yellow
  • B Resin: Liquid, Clear

Operating Steps

  1. Preheat the Master Mold: Heat the mold to 50-60 degrees Celsius and apply a release agent.
  2. Mix Resin A and B: Measure A and B resins according to the ratio, mix well, then vacuum for 90-120 seconds.
  3. Pour into Mold: Slowly pour the vacuumed mixture into the prepared mold.
  4. Curing: After the reaction, place in an oven at 80-100 degrees Celsius and cure for 1 hour.

Technical Parameters

  • Weight Ratio:

    • A : B = 100:140  by weight (CastSil 2002)
    • A : B = 100:100  by weight (CastSil 6502)
  • Reaction Time: 5 minutes (at 40°C)

  • Hardness: 20 (CastSil 2002), 65 (CastSil 6502)

  • Tear Resistance: OK

  • Color: Translucent Yellow

  • Shrinkage Rate: 0.3%-0.6%

 